In the context of wood drying, delamination can be regarded as a defect due to poor drying where separation between wood fiber cells occurs on surface (surface checks) or inside of wooden boards (internal checks) and in the form of splits (i.e. end split) at the end of the timber board. Solid wooden board can be considered as naturally laminated product. Before discussing delamination aspect of wood fibers during drying in further detail, it is helpful to discuss about basic principles and purpose of wood drying.

References


  1. Booker R, Koga S (2003) How collapse and internal checking happen in boards during drying. Wood processing newsletter 33, July 2003. New Zealand Forest Research Institute, RotoruaGoogle Scholar
  2. Desch HE, Dinwoodie JM (1996) Timber: Structure, properties, conversion and use. 7th edn. Macmillan Press, London, 306pGoogle Scholar
  3. Haque MN (1997) The chemical modification of wood with acetic anhydride. MSc Dissertation. The University of Wales, Bangor, 99pGoogle Scholar
  4. Haque MN (2002) Modelling of solar kilns and the development of an optimised schedule for drying hardwood timber. The University of Sydney, Australia, 354pGoogle Scholar
  5. Haque MN (2007) Simulation of temperature and moisture content profiles in a Pinus radiata board during high-temperature drying. Drying Technol 25(4):547–555CrossRefGoogle Scholar
  6. Innes T (1996) Improving seasoned hardwood timber quality with particular reference to collapse. PhD Thesis, University of Tasmania, Australia, 172pGoogle Scholar
  7. Keey RB, Langrish TAG, Walker,JCF (2000) Kiln-Drying of lumber. Springer, Berlin, 326pGoogle Scholar
  8. Kollmann, FFP, Cote WA Jr. (1968) Principles of wood science and technology. I. Solid Wood. Springer, NewYork, NY, 592pGoogle Scholar
  9. Kumar S (1994) Chemical modification of wood. Wood and Fiber Sci 26(2):270–280Google Scholar
  10. Pang S, Haslett AN (1995) The application of mathematical models to the commercial high-temperature drying of softwood lumber. Drying Technol 13(8–9), 1635–1674CrossRefGoogle Scholar
  11. Pordage LJ, Langrish, TAG (1999) Simulation of the effect of air velocity in the drying of hardwood timber. Drying Technol 17(1–2):237–256CrossRefGoogle Scholar
  12. Rowell RM (1983) Chemical modification of wood. For Prod Abstr 6(12):363–382Google Scholar
  13. Rowell RM (1991) Chemical modification of wood. In: Hon D.N.-S, Shiraishi N (eds) Wood and cellulosic chemistry, pp 703–756, Marcel Dekker, New York, NYGoogle Scholar
  14. Siau, JF (1984) Transport processes in wood. Springer, NewYork, NY 245pGoogle Scholar
  15. Stamm AJ (1964) Wood and cellulose science. Ronald Press, New York, NY, 509pGoogle Scholar
  16. Standard Australia (2001). Timber – assessment of drying quality. Australian/New Zealand Standard (AS/NZS) 4787, Sydney, 24pGoogle Scholar
  17. Vermass HF (1995) Drying eucalypts for quality: material characterstics, pre-drying treatments, drying methods, schedules and optimisation of drying quality. S Afr For J, 174:41–49Google Scholar
  18. Walker JCF, Butterfield BG, Langrish TAG, Harris JM, Uprichard JM (1993) Primary wood processing. Chapman and Hall, London, 595pGoogle Scholar
For further derails log on website :
https://link.springer.com/chapter/10.1007/978-90-481-9550-3_10

No comments:

Post a Comment

Advantages and Disadvantages of Fasting for Runners

Author BY   ANDREA CESPEDES  Food is fuel, especially for serious runners who need a lot of energy. It may seem counterintuiti...