Abstract

The effects of copper monoethanolamine (CuA) treatment of wood surfaces on the surface weathering and durability of a semitransparent penetrating stain were compared with those of chromic acid (CrA) treatment which is known as a photoprotective primer, using artificial weathering trials. Chemical changes in chemically treated and untreated wood surfaces during artificial weathering were investigated using Fourier transform infrared (FTIR) spectroscopy. Surface roughness, water contact angle measurements and scanning electron microscopy observations were performed to assess stain durability. Results of FTIR analyses indicated that lignin losses following CuA and CrA treatment were less than those of the untreated wood surfaces during the initial stage of artificial weathering. CuA pretreatment prior to staining also retarded the increase in the average surface roughness compared with that observed for the CrA-pretreated surface and untreated control (only stained) during artificial weathering. Furthermore, CuA pretreatment retarded the decrease in the contact angle compared with that observed for the untreated control, although the use of a highly concentrated CuA solution led to a decrease in the water repellency of the stained wood surface. These results indicated that CuA solution could be used for the pretreatment of wood surfaces to enhance the durability of semitransparent penetrating stains, as long as excessive CuA concentrations are avoided.

References

  1. Anderson EL, Pawlak Z, Owen NL, Feist WC (1991) Infrared studies of wood weathering. Part I: softwood. Appl Spectrosc 45(4):641–647CrossRef
  2. Baur SI, Easteal AJ (2014) ESR studies on the free radical generation in wood by irradiation with selected sources from UV to IR wavelength regions. Holzforschung 68:775–780CrossRef
  3. Black JM, Mraz EA (1974) Inorganic surface treatments for weather-resistant natural finishes. USDA For Serv Res Pap FPL 232:1–40
  4. Chang ST, Wang SY, Su YC (1998) Retention of red color in Taiwania (Taiwania Cryptomeriodes Hay.) heartwood. Holzforschung 52:13–17CrossRef
  5. Collier WE, Schultz TP, Kalasinsky VF (1992) Infrared study of lignin: reexamination of aryl-alkyl ether C–O stretching peak assignments. Holzforschung 46:523–528CrossRef
  6. Cornfield JA, Hale M, Fettis G (1994) A comparison of analytical and visual techniques used for assessment of weathering properties of chromium and copper azole treated timber. Int Res Gr Wood Preserv IRG/WP 94–20023
  7. Craciun R, Kamdem PD (1997) XPS and FTIR applied to the study of waterborne copper naphthenate wood preservatives. Holzforschung 51:207–213CrossRef
  8. Dawson BSW, Singh AP, Kroese HW, Schwitzer MA, Gallagher S, Riddiough SJ, Wu S (2008) Enhancing exterior performance of clear coatings through photostabilization of wood. Part 2: coating and weathering performance. J Coat Technol Res 5:207–219CrossRef
  9. Degroot WF (1985) Preliminary investigation of the association of inorganic cations with carboxylic acid groups in wood. Carbohydr Res 142:172–178CrossRef
  10. Deka M, Humar M, Rep G, Kričej B, Šentjurc M, Petrič M (2008) Effects of UV light irradiation on colour stability of thermally modified, copper ethanolamine treated and non-modified wood: EPR and DRIFT spectroscopic studies. Wood Sci Technol 42:5–20CrossRef
  11. Ebe K, Kataoka Y, Kiguchi M (2011) Evaluation of weatherability of finished wood by surface roughness. Mokuzai Hozon 37:122–129 (in Japanese with English summary) CrossRef
  12. Evans PD, Schmalzl KJ (1989) A quantitative weathering study of wood surfaces modified by chromium VI and iron III compounds. Part 1. loss in zero-span tensile strength and weight of thin wood veneers. Holzforschung 43:289–292CrossRef
  13. Evans PD, Michell AJ, Schmalzl KJ (1992) Studies of the degradation and protection of wood surfaces. Wood Sci Technol 26:151–163CrossRef
  14. Evans PD, Thay PD, Schmalzl KJ (1996) Degradation of wood surfaces during natural weathering. Effects on lignin and cellulose and on the adhesion of acrylic latex primers. Wood Sci Technol 30:411–422CrossRef
  15. Evans PD, Owen NL, Schmid S, Webster RD (2002) Weathering and photostability of benzoylated wood. Polym Degrad Stab 76:291–303CrossRef
  16. Feist WC (1988) Role of pigment concentration in the weathering of semitransparent stains. For Prod J 38:41–44
  17. Grelier S, Castellan A, Kamdem D (2000) Photoprotection of copper-amine-treated pine. Wood Fiber Sci 32:196–202
  18. Grüll G, Tscherne F, Spitaler I, Forsthuber B (2014) Comparison of wood coating durability in natural weathering and artificial weathering using fluorescent UV-lamps and water. Eur J Wood Wood Prod 72:367–376CrossRef
  19. Harrington KJ, Higgins HG, Michell AJ (1964) Inflared spectra of Eucalyptus regnans F. Muell. and Pinus radiata D. Don. Holzforschung 18:108–113CrossRef
  20. Hon DNS, Chang ST (1985) Photoprotection of wood surfaces by wood-ion complexes. Wood Fiber Sci 17(1):92–100
  21. Isaji S (2015) Correlation between natural and accelerated weathering of coated wood used in a cold region. J Japan Coat Technol Assoc 50:44–53 (in Japanese with English abstract)
  22. JIS B 0601 (2013) Geometrical product specifications (GPS) -surface texture: profile method-terms, definitions and surface texture parameters. Japanese Standard Association, Tokyo (in Japanese)
  23. JIS K 5600-7-7 (2008) Testing methods for paints-Part 7: Long-period performance of film- Section 7: Accelerated weathering and exposure to artificial radiation (Exposure to filtered xenon-arc radiation). Japanese Standard Association, Tokyo (in Japanese)
  24. Kamdem DP, Grelier S (2002) Surface roughness and color change of copper-amine treated red maple (Acer rubrum) exposed to artificial ultraviolet light. Holzforschung 56:473–478CrossRef
  25. Kataoka Y, Ishikawa A, Kobayashi M, Matsunaga M, Matsunaga H, Kiguchi M (2015) Weatherability of sugi (Cryptomeria japonica D. Don) sound barriers -Enhanced performance of coatings applied on preservative-treated wood-(in Japanese with English abstract). Mokuzai Hozon 41:62–70CrossRef
  26. Kiguchi M, Kataoka Y, Doi S, Mori M, Hasegawa M, Morita S, Kinjo M, Kadegaru Y, Imamura Y (1996) Evaluation of weathering resistance of the commercial pigmented stains by outdoor exposure test in Japan. Mokuzai Hozon 22:150–158 (in Japanese with English summary) CrossRef
  27. Kiguchi M, Kataoka Y, Doi S, Mori M, Hasegawa M, Morita S, Kinjo M, Kadegaru Y, Imamura Y (1997) Improvement of weather resistance of film-forming type clear finishes by pre-treatment with PEG and influence of exposure test sites. Mokuzai Hozon 23(4):168–175 (in Japanese with English summary) CrossRef
  28. Kiguchi M, Evans P, Ekstedt J, Williams R, Kataoka Y (2001) Improvement of the durability of clear coatings by grafting of UV-absorbers on to wood. Surf Coat Int Part B Coat Trans 84:263–270CrossRef
  29. Liu R, Ruddick JNR, Jin L (1994) The influence of copper (II) chemicals on the weathering of treated wood, Part I. ACQ treatment of wood on weathering. Int Res Gr Wood Preserv IRG/WP94-30040
  30. Michell AJ (1993) FTIR spectroscopic studies of the reactions of wood and of lignin model compounds with inorganic agents. Wood Sci Technol 27:69–80
  31. Nejad M, Cooper P (2011) Exterior wood coatings. Part-1: performance of semitransparent stains on preservative-treated wood. J Coat Technol Res 8:449–458CrossRef
  32. Ohtani K (1987) Chromium trioxide enhances the durability of wood doors. Chromium Rev 8:4–7
  33. Olsson SK, Johansson M, Westin M, Östmark E (2014) Reactive UV-absorber and epoxy functionalized soybean oil for enhanced UV-protection of clear coated wood. Polym Degrad Stab 110:405–414CrossRef
  34. Pandey KK, Khali DP (1998) Accelerated weathering of wood surfaces modified by chromium trioxide. Holzforschung 52:467–471CrossRef
  35. Pandey KK, Srinivas K (2014) Performance of polyurethane coatings on acetylated and benzoylated rubberwood. Eur J Wood Wood Prod 73:111–120CrossRef
  36. Rasti F, Scott G (1980) Mechanisms of antioxidant action: the role of copper salts in the photostabilization paint media. Eur Polym J 16:1153–1158CrossRef
  37. Ruddick JNR, Xie C, Herring FG (2001) Fixation of amine copper preservatives. Part 1. Reaction of vanillin, a lignin model compound with monoethanolamine copper sulphate solution. Holzforschung 55:129–133CrossRef
  38. Schaller C, Rogez D (2007) New approaches in wood coating stabilization. J Coat Technol Res 4(4):401–409CrossRef
  39. Schmalzl KJ, Forsyth CM, Evans PD (1995) The reaction of guaiacol with iron III and chromium compounds VI as a model for surface modification. Wood Sci Technol 29:307–319CrossRef
  40. Schmalzl KJ, Forsyth CM, Evans PD (2003) Evidence for the formation of chromium (III) diphenoquinone complexes during oxidation of guaiacol and 2,6-dimethoxyphenol with chromic acid. Polym Degrad Stab 82:399–407CrossRef
  41. Tolvaj L, Faix O (1995) Artificial ageing of wood monitored by DRIFT spectroscopy and CIE L*a*b* color measurements. 1. Effect of UV light. Holzforschung 49:397–404CrossRef
  42. Vollmer S, Evans PD (2013) Performance of clear coatings on modified wood exposed to the weather for 2 years in Australia. Int Wood Prod J 4(3):177–182CrossRef
  43. Weldon DG (2009) Failure analysis of paints and coatings. Wiley, New York p362
  44. Williams RS, Feist WC (1984) Application of ESCA to evaluate wood and cellulose surfaces modified by aqueous chromium trioxide treatment. Colloids Surf 9:253–271CrossRef
  45. Williams RS, Feist WC (1988) Performance of finishes on wood modified with chromium nitrate versus chromic acid. For Prod J 38:32–35
  46. Williams RS, Feist WC (1999) Selection and application of exterior stains for wood. General technical report FPL-GTR-106. USDA Forest service, Forest Products Laboratory, Madison
  47. Zhang J, Kamdem DP (2000) FTIR characterization of copper ethanolamine- wood interaction for wood preservation. Holzforschung 54:119–122
  48. Zhang J, Kamdem DP, Temiz A (2009) Weathering of copper-amine treated wood. Appl Surf Sci 256:842–846CrossRef


For further details log on website :
http://link.springer.com/article/10.1007/s00107-016-1078-2

No comments:

Post a Comment

Advantages and Disadvantages of Fasting for Runners

Author BY   ANDREA CESPEDES  Food is fuel, especially for serious runners who need a lot of energy. It may seem counterintuiti...