Published Date
Page 519-524 | Published online: 13 Apr 2010
Author
H. Ismail , A. M. Norjulia & Z. Ahmad
Abstract
Natural rubber compounds with untreated and treated kenaf were prepared with different loading i.e., 0, 10, 20, 30 and 40 phr. The compounds were cured at 150°C according to its cure time, t90. Curing characteristics, tensile properties, rubber-filler interaction and morphology properties of the rubber compounds were tested. Curing characteristics showed that scorch time, ts2 and cure time, t90 decreased with increasing of fibre loading and treatment. Mechanical properties of kenaf filled natural rubber compounds decreased with increasing of fibre loading but increased with fibre treatment. Swelling measurement and morphological study showed that better rubber-filler interaction was obtained with treated kenaf.
For further details log on website :
http://www.tandfonline.com/doi/full/10.1080/03602550903283117?src=recsys
Page 519-524 | Published online: 13 Apr 2010
Author
H. Ismail , A. M. Norjulia & Z. Ahmad
Abstract
Natural rubber compounds with untreated and treated kenaf were prepared with different loading i.e., 0, 10, 20, 30 and 40 phr. The compounds were cured at 150°C according to its cure time, t90. Curing characteristics, tensile properties, rubber-filler interaction and morphology properties of the rubber compounds were tested. Curing characteristics showed that scorch time, ts2 and cure time, t90 decreased with increasing of fibre loading and treatment. Mechanical properties of kenaf filled natural rubber compounds decreased with increasing of fibre loading but increased with fibre treatment. Swelling measurement and morphological study showed that better rubber-filler interaction was obtained with treated kenaf.
For further details log on website :
http://www.tandfonline.com/doi/full/10.1080/03602550903283117?src=recsys
No comments: